SM ISO690:2012 ШАРАГОВ, Василий. Повышение эксплуатационных свойств неорганических стекол выщелачиванием кислыми газами. In: Tehnocopia: revistă ştiinţifico-metodică, 2011, nr. 1(4), pp. 10-20. ISSN 1857-3843. |
EXPORT metadate: Google Scholar Crossref CERIF DataCite Dublin Core |
Tehnocopia: revistă ştiinţifico-metodică | ||||||
Numărul 1(4) / 2011 / ISSN 1857-3843 | ||||||
|
||||||
Pag. 10-20 | ||||||
|
||||||
Descarcă PDF | ||||||
Rezumat | ||||||
Thermochemical treatment by gases reagents in laboratory experiments increases water resistance of glass in 5 times, acid resistance – in 7 times, alkali resistance by 30 %, mechanical strength by 70 %, impact strength by 50 %, thermal stability and microhardness by 15 %. In industrial conditions the treatment with fluoride- and chlorine-containing reagents of industrial glasses for different purposes improves its chemical resistance by 1-2 orders, while the mechanical strength of glass increases by 30 %. Modification of sheet glass surface in industrial experiments is followed by an increase of its water resistance in 9 times, at this central symmetrical flexural strength grows by 30 %, the impact of strength increases by 20 %. |
||||||
Cuvinte-cheie стекло, выщелачивание, кислый газ, механическая прочность, термостойкость, микротвердость, химическая стойкость |
||||||
|
Cerif XML Export
<?xml version='1.0' encoding='utf-8'?> <CERIF xmlns='urn:xmlns:org:eurocris:cerif-1.5-1' xsi:schemaLocation='urn:xmlns:org:eurocris:cerif-1.5-1 http://www.eurocris.org/Uploads/Web%20pages/CERIF-1.5/CERIF_1.5_1.xsd' xmlns:xsi='http://www.w3.org/2001/XMLSchema-instance' release='1.5' date='2012-10-07' sourceDatabase='Output Profile'> <cfResPubl> <cfResPublId>ibn-ResPubl-26258</cfResPublId> <cfResPublDate>2011-01-04</cfResPublDate> <cfVol>4</cfVol> <cfIssue>1</cfIssue> <cfStartPage>10</cfStartPage> <cfISSN>1857-3843</cfISSN> <cfURI>https://ibn.idsi.md/ro/vizualizare_articol/26258</cfURI> <cfTitle cfLangCode='RU' cfTrans='o'>Повышение эксплуатационных свойств неорганических стекол выщелачиванием кислыми газами</cfTitle> <cfKeyw cfLangCode='RU' cfTrans='o'>стекло; выщелачивание; кислый газ; химическая стойкость; механическая прочность; термостойкость; микротвердость</cfKeyw> <cfAbstr cfLangCode='EN' cfTrans='o'>Thermochemical treatment by gases reagents in laboratory experiments increases water resistance of glass in 5 times, acid resistance – in 7 times, alkali resistance by 30 %, mechanical strength by 70 %, impact strength by 50 %, thermal stability and microhardness by 15 %. In industrial conditions the treatment with fluoride- and chlorine-containing reagents of industrial glasses for different purposes improves its chemical resistance by 1-2 orders, while the mechanical strength of glass increases by 30 %. Modification of sheet glass surface in industrial experiments is followed by an increase of its water resistance in 9 times, at this central symmetrical flexural strength grows by 30 %, the impact of strength increases by 20 %.</cfAbstr> <cfResPubl_Class> <cfClassId>eda2d9e9-34c5-11e1-b86c-0800200c9a66</cfClassId> <cfClassSchemeId>759af938-34ae-11e1-b86c-0800200c9a66</cfClassSchemeId> <cfStartDate>2011-01-04T24:00:00</cfStartDate> </cfResPubl_Class> <cfResPubl_Class> <cfClassId>e601872f-4b7e-4d88-929f-7df027b226c9</cfClassId> <cfClassSchemeId>40e90e2f-446d-460a-98e5-5dce57550c48</cfClassSchemeId> <cfStartDate>2011-01-04T24:00:00</cfStartDate> </cfResPubl_Class> <cfPers_ResPubl> <cfPersId>ibn-person-12173</cfPersId> <cfClassId>49815870-1cfe-11e1-8bc2-0800200c9a66</cfClassId> <cfClassSchemeId>b7135ad0-1d00-11e1-8bc2-0800200c9a66</cfClassSchemeId> <cfStartDate>2011-01-04T24:00:00</cfStartDate> </cfPers_ResPubl> </cfResPubl> <cfPers> <cfPersId>ibn-Pers-12173</cfPersId> <cfPersName_Pers> <cfPersNameId>ibn-PersName-12173-1</cfPersNameId> <cfClassId>55f90543-d631-42eb-8d47-d8d9266cbb26</cfClassId> <cfClassSchemeId>7375609d-cfa6-45ce-a803-75de69abe21f</cfClassSchemeId> <cfStartDate>2011-01-04T24:00:00</cfStartDate> <cfFamilyNames>Sharagov</cfFamilyNames> <cfFirstNames>Vasile</cfFirstNames> <cfFamilyNames>Шарагов</cfFamilyNames> <cfFirstNames>Василий</cfFirstNames> </cfPersName_Pers> </cfPers> </CERIF>